LMR600

Download the PDF document

2012-05-18 Print page

LMR600

Construction
Center Conductor: 4.47+0.01mm Bare Copper
Dielectric: 11.56+0.05mmFoam FPE
Shield: BONEDED Al Foil/TC Braiding
Braid Coverage: 90%TC
Jacket: 14.99mm PVC/PE
Jelly/APD Per Customers' Special Requirement
Characteristics
Sparker Test: 4000VAC  
Impedance: 50+2 Ohm  
Capacitance: 76.6pF/m  
Velocity of Propagation: 87%  
Return Loss: 20dB min (5-1000MHz)  
Attenuation  
Attenuation [@68o F. (20o C.)]  
Frequency (MHz) Maximum (dB/100 ft.)  
50 1.8  
150 3.2  
220 3.9  
450 5.6  
900 8.2  
1500 10.9  
1800 12.1  
2000 12.8  
2500 14.5  
5800 23.8